陕西兰盛钢铁资讯:方矩管壁厚允许偏差具体参照标准如下: 直缝电焊钢方管外径及壁厚允许偏差 GB/T13973 方矩管外径、壁厚的允许偏差 GB/T3091 无缝钢方管壁厚允许偏差 GB/T17395 冷拔或冷轧精密无缝钢方管规格及壁厚 GB/T3639 冷拔方方钢管规格尺寸及壁厚偏差GB/T3094 方管根据国标规定的允许的偏差厚度不同公差不一样。举例如下: 方矩管偏差等级: S1 允许偏差|0.1<S/D: ±15%,最小±0.6mm 允许偏差|0.05<S/D≤0.1: ±15%,最小±0.6mm 允许偏差|0.025<S/D≤0.05: ±15%,最小±0.6mm 允许偏差|S/D≤0.025: ±15%,最小±0.6mm偏差等级: 方矩管偏差等级: S2|A 允许偏差|0.1<S/D: ±12.5%,最小±0.4mm 允许偏差|0.05<S/D≤0.1: ±12.5%,最小±0.4mm 允许偏差|0.025<S/D≤0.05: ±12.5%,最小±0.4mm 允许偏差|S/D≤0.025: ±12.5%,最小±0.4mm 方矩管偏差等级: S2|B 允许偏差|0.1<S/D: +正偏差取决于重量要求,-12.5% 允许偏差|0.05<S/D≤0.1: +正偏差取决于重量要求,-12.5% 允许偏差|0.025<S/D≤0.05: +正偏差取决于重量要求,-12.5% 允许偏差|S/D≤0.025: +正偏差取决于重量要求,-12.5% 方矩管偏差等级: S3|A 允许偏差|0.1<S/D: ±10%,最小±0.2mm 允许偏差|0.05<S/D≤0.1: ±10%,最小±0.2mm 允许偏差|0.025<S/D≤0.05: ±10%,最小±0.2mm
允许偏差|S/D≤0.025: ±10%,最小±0.2mm
方矩管偏差等级: S3|B 允许偏差|0.1<S/D: ±10,最小0.4mm 允许偏差|0.05<S/D≤0.1: ±12.5,最小0.4mm 允许偏差|0.025<S/D≤0.05: ±12.5,最小0.4mm 允许偏差|S/D≤0.025: ±15,最小0.4mm
|